Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

Field Tests Show Pre-Painted Cut-Edge is More Durable Than Post-Painted

October 1, 2005
Photo 1/Post-paint 1.0-mil spray at 16 months.
Some manufacturers have shied away from using pre-painted metal parts when there is an exposed cut-edge in the design, for fear of corrosion. The National Coil Coating Association (NCCA) set out to put this misconception to the test. The NCCA, along with the help of PPG Industries, Inc., and the North American Zinc-Aluminum Coaters Association (NamZAC), worked together to compare the corrosion resistance of pre-painted metal louvers on air conditioning units to those coated with three types of post-paint.



Photo 2/Prepaint finish 1.0 mil at 16 months.
Pre-painted louvers with exposed cut edges were tested in the field alongside three sets of metal louvers, one with a post-painted electrocoat, a second with a powder finish and a third with a spray finish. The parts in all instances were made of hot-dipped galvanized steel; louvers were exposed to the same environment over time in Daytona Beach, FL.



Photo 3/Post-paint 1.0 mil electrocoat at 39 months.
Comparisons made after 16 months, 39 months, 44 months and 68 months of exposure to the elements showed pre-painted parts were repeatedly and significantly better than the post-painted parts in terms of the corrosion resistance, uniformity of treatment and film thickness.



Photo 4/Prepaint finish 1.0 mil at 39 months.
The reason that the pre-painted parts outperformed each of those with a post-painted application is due to the fact that pre-painted metal sheet is uniformly cleaned, pretreated and painted as a flat surface, so the edge-to-edge and side-to-side variability is virtually eliminated. In addition, the pre-painted part also has two coats of paint, tightly bonded to the metal as compared to a post-painted part, which generally has only one coat of paint. In most cases, the pre-painted part has paint (one or two coats) on the backside as compared to the post-painted part, which at best has a minimal amount of overspray. Uniform pretreatment and paint on the backside of a part increases the corrosion resistance of the part, enhancing long-term durability. This can be seen in Photos 1 and 2.



Photo 5/Post-painted with 1.0-mil spray at 68 months.
Cut or sheared edges expose the metal to the environment, thereby creating a reactive area at which corrosion can begin. The degree to which corrosion will occur depends on the type of metal, the thickness of the sheet, the pretreatment system and uniformity, the paint system and thickness, application method and the environment, as well as the angle of exposure (vertical or horizontal).



Photo 6/Pre-painted finish with 1.0 mil at 68 months.
Areas where moisture is retained generally have the most severe corrosion. The moisture allows the ingress of contaminants (chemicals, salts, debris, etc.), which will attack the metal. The initial sign of corrosion is usually visible as microblistering on the surface of the painted panel/part. With time, this microblistering causes the paint to creep back from the cut edge. The pretreated metal is exposed as the paint creeps back. The pretreatment is the final defense for corrosion resistance.



Photo 7/Post-painted with 1.0-mil spray at 68 months.
The enhanced corrosion resistance observed when using pre-painted sheet as compared to other post-painted methods of application is so significant, that in many cases metallic coating weights may be reduced.

Photo 8/Pre-painted finish with 1.0 mil at 68 months.
Once corrosion has been initiated, it usually continues at a steady rate, progressing through a metallic coating (if present) and into the metal (Photos 3 and 4).

The study findings conclude that cut edge protection of pre-painted parts has repeatedly proven to be significantly better than post-painted ones because of the uniformity of treatment and film thickness (Photos 5-8). With proper selection of paint and substrate, a pre-painted part should provide a superior, cost-effective product in corrosion resistance, appearance and durability as compared to parts painted using other paint application methods.

For more information about this study, or converting to pre-painted metal, visit www.coilcoatinginstitute.org or call the NCCA at 216/241.7333.

About Pre-Painted Metal

Pre-painted metal sheet has touched every aspect of daily life over the past 30 years. Its versatility allows it to be used almost everywhere - on building exteriors and interiors, appliances, HVAC, furniture, automotive, etc. It is functional and durable, and can be combined with high-performance paint systems with an unlimited spectrum of colors and an array of properties. Designs can be eye appealing - simple or complex - without affecting long-term durability, corrosion and mar resistance, or functionality.

These conversions to cost-effective, quality-enhanced pre-painted products occur almost daily from costly, labor-intensive and inefficient post-paint systems (electrocoat, spray and powder). Long-term durability is a key property of any painted metal product. In particular, protection of a cut or exposed edge is critical, no matter what type of paint application method.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Paint and Coating Market Reports
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • Emerald Featuring Innovative Performance Materials for Tougher, More Durable Coatings

    See More
  • did you know column

    Creating Core-Shell Latex Particles is Sometimes More a Dream than Reality

    See More
  • Steelscape Offers Pre-Painted Steel With Graffiti-Resistant Coatings

    See More

Related Products

See More Products
  • pci march 2020

    PCI March 2020 Issue

  • Handbook of Adhesives and Sealants, Volume 1

  • pci may 2020

    PCI May 2020 Issue

See More Products

Related Directories

  • Atlas Material Testing Technology LLC

    For more than 100 years, Atlas has been a leader in materials testing, offering a complete line of weathering testing instrumentation, laboratory, and outdoor testing services.
  • Titan

    As a leader in spraying technology, Titan manufactures and markets a full line of professional-grade paint sprayers for applying a variety of coatings.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing