Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Industrial CoatingsSpecial Purpose CoatingsFormulating with Mike

Self-Leveling Coatings: Formulating Tips

By Mike Praw, Technical Service & Development Manager – Coatings and Performance Products, Indorama Ventures, The Woodlands, TX
pci0423-Formulating-874157664-1170.jpg

Davizro / iStock / Getty Images Plus, via Getty Images.

June 4, 2025

In previous columns, we discussed self-leveling coatings, with a focus on 100% active polyurethane systems. In this month’s column, we will discuss formulating tips for these systems.

The advantage of 100% active self-leveling urethane coatings based on methylene diphenyl diisocyanate (MDI) is the low viscosity, good physical properties of the coatings and relatively low cost. These systems can be formulated to have the same compression strength and Shore D hardness of epoxy systems, but still have about three times the elongation at break and twice the Taber abrasion resistance. This allows them to be crack bridging. The disadvantage of these systems is that the MDI will readily react with water to form polyurea and CO₂. The evolution of the gas can cause foam issues in the coating.

Most self-leveling coatings go over concrete, and this concrete will normally contain moisture. The best way to prevent the urethane from foaming is to use a primer/sealer such as a two-component (2K) epoxy. Once the substrate is sealed to stop water from encountering the urethane, the next place for moisture to contact the coating is from raw materials in the coating. Therefore, it is necessary to use low water-containing urethane-grade raw materials. It is difficult to keep moisture out of some raw materials like pigments, so a moisture scavenger is added to the resin side of the 2K system. The most common is zeolite powder. Zeolite powder is nonreactive, has a high moisture adsorption capacity and works at low moisture levels, making it excellent for pigmented urethane systems. It is normally supplied as a powder or as a dispersion (normally ~50% in castor oil). Since it takes one to three days to adsorb the water through physical adsorption, you cannot make and use a coating right away and expect no bubbling. A good starting point is ~0.25–0.50% by weight of the resin side of the formula.

If the system is clear (such as for aliphatic topcoats) or you need to dewater raw materials for the isocyanate part of the 2K system, monomeric isocyanates can be used as moisture scavengers. Oxazolidine-based moisture scavengers react quickly with water, but like monomeric isocyanates, can have toxicological issues. Other liquid moisture scavengers include silanes that will also react with water.

Choice of the urethane catalyst (not normally needed for MDI, but required for aliphatic urethane systems) includes either gelling-type catalysts like triethylene diamine (TEDA) or organotin, or blowing catalysts like 2,2'-dimorpholinodiethylether (DMDEE). Gelling catalysts promote the urethane reaction over the urea reaction. Blowing catalysts promote the urea reaction over the urethane reaction. In coatings, only gelling catalysts are used since we want to minimize the water side reaction resulting in urea linkages.

For low-temperature application, catalysts can be used with MDI-based systems, but it is critical that the coating be at the low temperature during mixing to prevent too short a pot life. If longer pot life is needed, organic acids can help retard the urethane reaction.

Often polypropylene glycol (PPG) polyols are used with MDI, but there are compatibility issues between MDI and higher molecular weight PPGs. There are several ways to help compatibilize the two, including adding castor oil, ethylene diamine or toluene diamine-based PPG polyols, or by reacting the PPG polyol with ethylene oxide to create a polyethylene glycol end cap. As castor oil is often used in these systems, that is the preferred way to go.

Due to the low viscosity of these systems, pigments will easily settle out. Adding an antisettling agent will be necessary. The key is to prevent settling without increasing viscosity to the point that the coating loses its self-leveling nature. Often, fumed silicas or clays are used to accomplish this.

Lowering gloss in self-leveling coatings is difficult and takes a large amount of pigment. Normally, hydrophilic pigments like calcium carbonate should be avoided to limit water in the coating. There is only so much moisture scavengers can do. Fumed silica for antisettling and zeolite for moisture scavenging will help lower gloss in addition to the extender pigments. Adding pigments will increase tensile strength and hardness but can hurt flexibility and elongation.

As a final note, MDI-based, self-leveling urethane systems are great for areas that are dimensionally less stable (such as concrete with cracks) or where high abrasion resistance is needed (parking decks, warehouses with forklift traffic). If high chemical resistance is needed, epoxy systems can provide it. If UV resistance is needed, an aliphatic topcoat is required.

 

All information contained herein is provided "as is" without any warranties, express or implied, and under no circumstances shall the author or Indorama be liable for any damages of any nature whatsoever resulting from the use or reliance upon such information. Nothing contained in this publication should be construed as a license under any intellectual property right of any entity, or as a suggestion, recommendation, or authorization to take any action that would infringe any patent. The term "Indorama" is used herein for convenience only, and refers to Indorama Ventures Oxides LLC, its direct and indirect affiliates, and their employees, officers and directors.

KEYWORDS: Concrete Coatings Floor Coatings formulating tips Low-VOC Paint and Coatings plasticizers

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Mike Praw, Technical Service & Development Manager – Coatings and Performance Products, Indorama Ventures, The Woodlands, TX

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • colorful building exterior
    Sponsored byDow

    Insights into Exterior Architectural Coating Degradation: Bridging Accelerated and Natural Weathering

  • digital pigments
    Sponsored bySiltech

    The Fourth Dimension of Silicon: Siltech Q Resins

Popular Stories

Company News

What the AkzoNobel–Axalta Merger Means for the Future of Coatings

AkzoNobel and Axalta Headquarters

AkzoNobel and Axalta Announce $25 Billion Merger

Wacker logo

WACKER Plans More Than 1,500 Job Cuts



PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

March 24, 2026

The Manufacturing & Automation eXchange (MAX)

MAX presents a rare opportunity to observe the full scope of manufacturing in one environment. From systems integration and materials handling to automation, quality, safety, and packaging, each discipline is represented through live, operational displays. By experiencing these technologies side by side, as they are on actual production floors, attendees gain a grounded understanding of how manufacturing functions align, overlap, and evolve in practice.

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
pci voices from the top ebook

PCI webinar

Related Articles

  • pci0423-Formulating-874157664-1170.jpg

    The Role of Self-Leveling Coatings

    See More
  • pci0423-Formulating-874157664-1170.jpg

    Self-Leveling Coatings: Polyols for Urethanes

    See More
  • Bio-Based Solution for Self-Leveling Coatings

    See More

Related Products

See More Products
  • Formulating for Architectural Coatings (Virtual Course - 5/21/26)

See More Products

Related Directories

  • Formulator Software LLC

    At Formulator Software, we understand the precision and complexity involved in perfecting formulations. Our software is designed specifically for chemists, lab technicians, researchers, and manufacturers, providing essential tools to streamline the entire formulation process. Formed in 2002, Formulator Software is trusted by thousands to manage their raw materials, formulations, QC, SDS, COA, costing and more!
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2025. All Rights Reserved BNP Media.

Design, CMS, Hosting & Web Development :: ePublishing