Appleton to Microencapsulate Biocides for Troy Corp.

APPLETON, WI - Encapsys®, the microencapsulation division of Appleton Papers, has entered into an exclusive strategic partnership with Troy Corp., Florham Park, NJ, to develop and supply a microencapsulated biocide to select marketplaces worldwide.

Encapsys scientists relied on an innovative, joint development agreement with Troy to create a custom-formulated microencapsulation system that provides a controlled release mechanism for specialty biocide additives. Through microencapsulation, Encapsys scientists were able to control the antimicrobial activity of a biocide to be used in paints, architectural coatings and mortar formulations.

The microencapsulation process, Microencapsulation, is the process in which solid, liquid or gaseous core materials are encased in “shells” or “capsules” that are one micron to several hundred microns in diameter. Among the many benefits of microencapsulation is the controlled release of a core material.

“We use an open, collaborative approach with our partners that enables us to deliver effective and rapid product innovations that none of us would likely achieve on our own,” said Steve Wilhelms, General Manager of Encapsys. “We relied on the product knowledge and market insight of the Troy team, and they relied on the depth and breadth of our technical expertise to deliver a unique application of microencapsulation technology. And we did so in just 18 months.”

Appleton scientists and engineers started working with microencapsulation in 1954 when the NCR scientists who invented and patented the process approached Appleton to develop a workable microcapular coating that would lead to the introduction of carbonless paper. Appleton scientists have continued to develop and refine microencapsulation technology and explore the potential for microencapsulation to extend to applications beyond carbonless paper. Those efforts have enabled Appleton to develop specific and proprietary product solutions for the consumer products industry, which led to the creation of Appleton’s Encapsys division.
You must register or login in order to post comments.

Multimedia

Videos

Image Galleries

American Coating Show 2012

The American Coatings Show and Conference, held every two years, took place May 7-10 at the Indiana Convention Center in Indianapolis, IN, in the heart of the Manufacturing Belt, the oldest and largest concentration of industrial companies in the Midwest.

Podcasts

PCI Top 5 - January 12, 2012
PCI's Podcast series on the five most e-mailed/shared articles and stories for the week.

More Podcasts

THE MAGAZINE

PCI Magazine

PCI may 2012 cover

2012 May

Check out PCI's May issue!!

TABLE OF CONTENTS SUBSCRIBE

iPad

Do you own/use an iPad?
If yes, do you use your iPad for business or personal reasons?
Have you purchased a business app within the last 6 months?
See Poll Results Poll Archive

THE PCI STORE

PCI-June-2011-Coversmall.gif
PCI Additives Handbook

Encyclopedia of information on the properties and uses of coatings additives.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Virtual Brochures

PageCollageClick on the Virtual Brochures page to view multiple categories that list downloadable product literature from leading industry suppliers.

STAY CONNECTED

Facebook Twitter  LinkedIn YouTube