W. CONSHOHOCKEN, PA – A new ASTM guide standardizes a useful, fast and easy technique for collecting infrared spectra of non-aqueous liquid paints right out of the can. The new standard, ASTM D 7588, Guide for FT-IR Fingerprinting of a Non-Aqueous Liquid Paint as Supplied in the Manufacturer’s Container, is under the jurisdiction of Subcommittee D01.21 on Chemical Analysis of Paints and Paint Materials, which is part of ASTM International Committee D01 on Paint and Related Coatings, Materials and Applications.

The new guide will be useful for quality, formula and process control, failure analysis, chemical identification, and compositional and raw material comparisons.

A new standard, ASTM G 207, Test Method for Indoor Transfer of Calibration from Reference to Field Pyranometers, was developed by Subcommittee G03.09 on Radiometry, part of ASTM International Committee G03 on Weathering and Durability. ASTM G 207 facilitates calibration of solar sensors used in accelerated testing under simulated sunlight and outdoor weathering tests as well as performance monitoring of solar energy conversion systems.

You must register or login in order to post comments.

Multimedia

Videos

Image Galleries

American Coating Show 2012

The American Coatings Show and Conference, held every two years, took place May 7-10 at the Indiana Convention Center in Indianapolis, IN, in the heart of the Manufacturing Belt, the oldest and largest concentration of industrial companies in the Midwest.

Podcasts

PCI Top 5 - January 12, 2012
PCI's Podcast series on the five most e-mailed/shared articles and stories for the week.

More Podcasts

THE MAGAZINE

PCI Magazine

PCI may 2012 cover

2012 May

Check out PCI's May issue!!

TABLE OF CONTENTS SUBSCRIBE

iPad

Do you own/use an iPad?
If yes, do you use your iPad for business or personal reasons?
Have you purchased a business app within the last 6 months?
See Poll Results Poll Archive

THE PCI STORE

PCI-June-2011-Coversmall.gif
PCI Additives Handbook

Encyclopedia of information on the properties and uses of coatings additives.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Virtual Brochures

PageCollageClick on the Virtual Brochures page to view multiple categories that list downloadable product literature from leading industry suppliers.

STAY CONNECTED

Facebook Twitter  LinkedIn YouTube