WEST CONSHOHOCKEN, PA — ASTM has announced a major change in its Standard Test Method for Scrub Resistance of Wall Paints (ASTM D 2486), a procedure that determines the resistance of wall paint to erosion caused by scrubbing.

In the standard’s newly introduced “Method B,” two paints are drawn down simultaneously, with one of the paints serving as a “control,” or reference paint. The test method was revised by ASTM Subcommittee D01.42 on Architectural Coatings in a project led by Thomas Sliva of DL Laboratories. ASTM standards are available from the organization’s customer service department at 610/832.9585; e-mail service@astm.org, or website store at www.astm.org. More information also is available from Sliva at DL Labs, 212/777.4445; e-mail dllabs@aol.com.

ASTM also announced plans for a mini-symposium, “New Developments in Paint Testing Instruments,” on Jan. 23, 2001, in Fort Lauderdale, FL. The symposium, to be held in conjunction with the ASTM’s semi-annual meeting, will examine areas that should be considered for development or improvement of testing methods, the organization said. Suppliers of coatings test instruments will review testing methods and equipment that they are proposing for consideration by ASTM Committee D01 on Paint and Related Coatings, Materials, and Applications.

The symposium is free of charge. More information can be obtained from symposium chairman Joe Peters, Leneta Co., at 201/847.9300; e-mail jpeters@leneta.com. More information on ASTM Committee D01 can be obtained from Tim Brooke, ASTM, at 610/832.9729; e-mail tbrooke@astm.org.

Links

You must register or login in order to post comments.

Multimedia

Videos

Image Galleries

American Coating Show 2012

The American Coatings Show and Conference, held every two years, took place May 7-10 at the Indiana Convention Center in Indianapolis, IN, in the heart of the Manufacturing Belt, the oldest and largest concentration of industrial companies in the Midwest.

Podcasts

PCI Top 5 - January 12, 2012
PCI's Podcast series on the five most e-mailed/shared articles and stories for the week.

More Podcasts

THE MAGAZINE

PCI Magazine

PCI may 2012 cover

2012 May

Check out PCI's May issue!!

TABLE OF CONTENTS SUBSCRIBE

iPad

Do you own/use an iPad?
If yes, do you use your iPad for business or personal reasons?
Have you purchased a business app within the last 6 months?
See Poll Results Poll Archive

THE PCI STORE

PCI-June-2011-Coversmall.gif
PCI Additives Handbook

Encyclopedia of information on the properties and uses of coatings additives.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Virtual Brochures

PageCollageClick on the Virtual Brochures page to view multiple categories that list downloadable product literature from leading industry suppliers.

STAY CONNECTED

Facebook Twitter  LinkedIn YouTube