Daimler Chooses GREENKOTE Coating Process

GREENKOTE® Plc, a global coating technology company headquartered in Cleveland, will provide corrosion protection for selected Daimler automotive parts beginning in the first half of 2010. I

CLEVELAND - GREENKOTE® Plc, a global coating technology company headquartered in Cleveland, will provide corrosion protection for selected Daimler automotive parts beginning in the first half of 2010. Initial orders include components for passenger-safety-related applications. Additionally, the automotive industry giant is finalizing technical approval of GREENKOTE as one of its suppliers of zinc diffusion coatings, using the company’s patented Thermo-Diffusion coating process.
 
The decision by Daimler to use GREENKOTE zinc thermal diffusion coating protection comes after nearly two years of testing zinc diffusion systems and topcoat on its products, especially those most sensitive to corrosion. The extensive testing involved mostly small screws, with more than 10 potential products identified to undergo the duplex coating process. Other small parts include fasteners, fixtures, screws, nuts and some critical wiper parts on several of Daimler’s automotive platforms including Limousine E-Class and S-Class vehicles.
 
GREENKOTE is a thermal diffusion coatings process that modifies and improves the basic surface characteristics of metals and is applicable to metal finished parts in many industries including automotive.
You must register or login in order to post comments.

Multimedia

Videos

Image Galleries

American Coating Show 2012

The American Coatings Show and Conference, held every two years, took place May 7-10 at the Indiana Convention Center in Indianapolis, IN, in the heart of the Manufacturing Belt, the oldest and largest concentration of industrial companies in the Midwest.

Podcasts

PCI Top 5 - January 12, 2012
PCI's Podcast series on the five most e-mailed/shared articles and stories for the week.

More Podcasts

THE MAGAZINE

PCI Magazine

PCI may 2012 cover

2012 May

Check out PCI's May issue!!

TABLE OF CONTENTS SUBSCRIBE

iPad

Do you own/use an iPad?
If yes, do you use your iPad for business or personal reasons?
Have you purchased a business app within the last 6 months?
See Poll Results Poll Archive

THE PCI STORE

PCI-June-2011-Coversmall.gif
PCI Additives Handbook

Encyclopedia of information on the properties and uses of coatings additives.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Virtual Brochures

PageCollageClick on the Virtual Brochures page to view multiple categories that list downloadable product literature from leading industry suppliers.

STAY CONNECTED

Facebook Twitter  LinkedIn YouTube