Engelhard offers Mearlin® Firemist™ pigments.
Engelhard Corp. offers Mearlin® Firemist™ pigments, which are patented borosilicate-based pigments that can go beyond traditional pearlescent pigments in chroma, color purity, brightness, transparency and reflectivity. Applications include automotive, motorcycle, bicycle, decorative and gel-coat coatings.
Engelhard Corp. offers Mearlin® Firemist™ pigments, which are patented borosilicate-based pigments that can go beyond traditional pearlescent pigments in chroma, color purity, brightness, transparency and reflectivity. Applications include automotive, motorcycle, bicycle, decorative and gel-coat coatings.