Johnson Matthey has made available Timbasol™ solvent-based dispersions. The materials are transparent iron oxide and carbon black pigments for natural wood shade formulations. A range of organic and inorganic pigments is available for decorative fashion colors and natural shade tinting. The resins are long oil alkyd based, and the solvents are white spirit/hydrocarbon distillate.