HALOX: The HALOX® 900 water-based, nitrite-free temporary corrosion inhibitor is formulated with a patented technological chemistry to offer corrosion protection for both ferrous and non-ferrous metals. In addition to providing temporary rust protection to bare metal, the product also promotes adhesion of the coating to the substrate. The rust protection lasts from days to months, depending on exposure conditions. Call 219.933.1560 or visit www.halox.com.