Permeability Identified as a Critical Corrosion Factor (11/22/06)

According to an independent survey of wastewater engineers, municipal managers and contractors, a chemically resistant lining's permeability to corrosive substances was shown to be the most important consideration during product selection. The survey was conducted in April 2006 by WaterOnline, a service for the water and wastewater industry, and was sponsored by Sauereisen, Inc., a manufacturer of industrial construction materials.

"Because of government mandated industrial pretreatment, longer detention times for waste water due to air quality regulations and other factors, concrete structures in waste water infrastructure are exposed to more severe conditions now than in the past," said Randy Nixon, senior consultant, Corrosion Probe, Inc., an engineering and consulting firm in the field of corrosion and material science. "Under these conditions, permeability is perhaps the most prominent factor in the failure of coatings designed to protect concrete from this rapid degradation."

Although approximately 70% of those surveyed said permeability to corrosive substances is the most critical factor for chemically resistant linings, more than 64% said permeability is the most commonly overlooked aspect of corrosion-resistant lining selection. The study also revealed chemical resistance to be the most important quality of protective linings, with porosity ranked as the number one factor in determining chemical resistance.

For more information, call 412.963.0303 or click on the website link below.

Links

You must register or login in order to post comments.

Multimedia

Videos

Image Galleries

American Coating Show 2012

The American Coatings Show and Conference, held every two years, took place May 7-10 at the Indiana Convention Center in Indianapolis, IN, in the heart of the Manufacturing Belt, the oldest and largest concentration of industrial companies in the Midwest.

Podcasts

PCI Top 5 - January 12, 2012
PCI's Podcast series on the five most e-mailed/shared articles and stories for the week.

More Podcasts

THE MAGAZINE

PCI Magazine

PCI may 2012 cover

2012 May

Check out PCI's May issue!!

TABLE OF CONTENTS SUBSCRIBE

iPad

Do you own/use an iPad?
If yes, do you use your iPad for business or personal reasons?
Have you purchased a business app within the last 6 months?
See Poll Results Poll Archive

THE PCI STORE

PCI-June-2011-Coversmall.gif
PCI Additives Handbook

Encyclopedia of information on the properties and uses of coatings additives.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Virtual Brochures

PageCollageClick on the Virtual Brochures page to view multiple categories that list downloadable product literature from leading industry suppliers.

STAY CONNECTED

Facebook Twitter  LinkedIn YouTube