Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

Pigment Blacks in Waterborne Coatings

January 1, 2002
The coatings industry grows at an annual rate of about 2%. Low-solvent or solvent-free coating systems are disproportionately growing at the expense of solvent-containing systems. Apart from powder coatings, high-solids and radiation-curing systems, environmentally friendly waterborne coatings are especially successful in industrialized countries.

This trend is being led by the automotive industry, which favors low-polluting coating systems. Aqueous-based paints are relatively quickly realizable alternatives. They are becoming well established not only in the field of OEM (original equipment manufacturers) but are also gaining in importance in the repair industry.

The increasingly strict environmental laws in Germany and the European Union require paint manufacturers to permanently allocate considerable adjustment expenditures. Not only is a decrease in emissions required, but applicability and the characteristics desired by the consumer must also be ensured. In this context, coloristic data demand special attention. Achieving the same jetness and hue in a new binder system is an essential development task.

This article will show a part of the experimental results obtained in the use of pigment blacks in various binders using approximately 10 additives. Although colloid chemistry experience in the field of waterborne paints is growing rapidly, a considerable part of what we know is still based on pure empirical knowledge. Work is exclusively focused on coloristic data. Other effects of additives on the paint must be studied separately.

The "Color" Black

In the true sense of the word, black is not a color that arises from the absorption of a specific wavelength of visible light and the reflection of the complementary color. A surface appears black whenever it reflects less than 1% of light. For the past 10 years, the popularity of black in the automobile industry has not diminished. Pigment blacks have proven their worth when it comes to jetness because they not only exceed the jetness of RAL 9005 (deep black), but they also achieve a blue-tinted blackness, which is perceived by the observer as particularly intense.

It was a big problem in coloristic characteristics to quantify the jetness and hue of black paints.

It is readily apparent - for best results, in the sun or under a focused beam of light - whether a paint film surface is more jet black, blue-tinged or brown-tinged than another. However, it was impossible to express this difference in numbers.

With the development of colorimetric devices that distinguish well particularly in lower reflection areas, it is now possible to precisely quantify hues in the reflection area of <1%. The My value is derived from the standardized coordinate Yn for the green portion of the CIELAB system (see Figures 1-2). With the integration of Xn (red) and Zn (blue), the overall color impression is shown. Consequently, it is mathematically relatively simple to calculate the color ratio dM.1-2

Table 1

Basic Characteristics
Production of Pigment Blacks

Pigment blacks are manufactured using three production processes: the gas black, furnace black and lamp black processes.4-5 Gas blacks have numerous "acidic" chemical groups on their particle surface while furnace blacks are weakly basic. Degussa gas blacks have an average primary particle size from 11 to 29 nm, and are characterized by their good dispersibility, as well as their solvent and binder compatibility. They have proven their worth worldwide in mass-tone coloration and as tinting pigments, and are preferred by numerous paint producers. Furnace and lamp blacks are used especially as tinting pigments.

Table 3

Particle Size and Jetness

The smaller the particles, the bigger its light absorption or the smaller the light reflection. At the same time, the finer the pigment black, the greater the jetness (see Figure 3). Thus, the primary particle size of the pigment black with identical carbon black concentration is the deciding factor in a paint's jetness.

The size of actually existing agglomerates determines the hue. When viewed from the top, small agglomerates in mass tone demonstrate a blue tint, while larger agglomerates usually show the less desired red tint. It is, therefore, necessary to stabilize agglomerates after intensive dispersion in such a way that they do not flocculate.

Table 4

Surface Modification

Oxidation of pigment blacks produces increased polar chemical groups on the particle surface area, which possess a higher affinity to the polar groups of paint binders. This especially applies to carboxyl groups. The treatment thus produces better dispersion and stabilization of the pigment black in the liquid phase and better distribution in a polymer matrix. In mass tone it yields a bluish tint.

Figure 1

Pigment Black Dispersion Grinding Process

The dispersion of pigments and fillers takes place in several steps, some of which run parallel. Schematically one can distinguish the incorporation and the wetting of agglomerates present in the powder, their mechanical division and the wetting and the stabilization of freed boundary surfaces, thereby preventing the recombination of fragments. Agglomerates stabilize overall through adsorption of binders or wetting agents, which hamper undesired flocculation.

The smallest possible agglomerates of the pigment black and the narrowest possible agglomerate size distribution in the corresponding coating system are essential to produce optimal coloristic results. Dispersion is influenced by many parameters, which shall be discussed later on.

Grinding Media

The usual grinding media for pearl mills, attritors, Skandex, Red Devil, etc., consist of various materials that differ from each other primarily by their density and hardness. Special attention should be paid, in particular, to the following.
    Glass -- approx. 1.5 g/cm3
    Porcelain -- approx. 3.0 g/cm3
    Steatite -- approx. 2.6 g/cm3
    Al-oxide -- approx. 3.5 g/cm3
    Zr-silicate -- approx. 3.9 g/cm3
    Steel -- approx. 3.9 g/cm3
With an increase of the specific weight, the energy intake by the system and consequently the dispersion effect also increase. When faced with high dispersion requirements, grinding balls with the highest possible density should be used. In the case of steel balls, however, a stronger temperature increase and a possible abrasion must be taken into account. Abrasion could influence the color or become catalytically active. Possible corrosion must also be considered.

Grinding Media Size

Grinding media with a smaller diameter have a positive effect on the dispersion of pigment blacks, although their separation and cleansing are more difficult to achieve. In the experiments that will be described later, grinding media with diameters from 0.6-0.8 or 1.6-2.0 mm were used. These are the same media that are used in practice by paint manufacturers.

Figure 2

Dispersion Time

The longer the dispersion time, the better the degree of dispersion, which manifests itself in a low grindometer value, a high tinting strength or jetness and reduced haze. Good dispersion in pigment blacks leads to grindometer values of less than 10. In connection with this, pigment stability and to a certain extent the blue hue, in mass tone coloring especially, increase. However, only certain limit values are ultimately achieved and these values are dependent on the dispersion aggregate and of course the paint system.

Wetting and Stabilization

As usual for fine pigments, the pigment black surface to be wetted and stabilized becomes larger with increasing dispersion. The developing reactive centers of the boundary surfaces must be saturated, i.e., stabilized and kept from re-agglomerating or flocculating. This requires adequate interaction of the dissolved or emusified paint constituents or the solvents with the pigment blacks. While in conventional systems this takes place through the adsorption of binder molecules and the resulting steric hindrance of the adsorbate, the electrostatic repulsion of the pigment particles or the corresponding adsorbates prevails in strongly polar systems such as waterborne paints. In general, the surface chemistry, the morphology and structure of the pigment black, the wetting capacity of the binder, the accompanying additives (wetting aids) as well as the solvents determine pigment black stabilization.

As a rule of thumb, the following applies in the evaluation of the coloristic characteristics of a black paint in the first approximation:

    blue undertone = good stability

    brown undertone = lacking in stability

Since pigment blacks differ in morphology, structure and surface chemistry, the optimal stabilization requirements must be determined for every pigment black (or at least for every pigment black class) in order to achieve the desired coloristic characteristics. In waterborne paints the decisive factors are the dispersion resin and the wetting agent(s).

In solventborne coatings it is possible to obtain good results without wetting agent, only by optimizing the grinding resins, the resin concentration and the solvents.

Waterborne Paints

Water as a solvent or emulsifying medium for paints differs fundamentally from organic solvents. Not only the inadequate wetting behavior or dissolving power for polymers, but also the high polarity and surface tension must be taken into account in the formulation of paints. Pigment blacks can be wetted with water but can hardly be stabilized. Therefore, polymers and wetting agents are of much greater importance here than in conventional systems.

For the dispersion of fine pigment blacks there are basically two ways to achieve success. First, carbon black is dispersed in water with the resin - if necessary - with small proportions of wetting and antifoam agents. Second, with no resin, pigment black is dispersed in a water/wetting agent mixture containing suitable antifoam agents and, if necessary, rheological additives.

Grinding with Dispersion Resins

Four different resins and three carbon blacks were evaluated.In order to determine the effect of the pure binder, no wetting agent was used. Results are shown in Table 2.

Stability of Paints with FW 285 and FW 200

The stability of two paints was tested every four weeks during a storage time of six months at room temperature. Coloristic data, pH and degree of gloss were determined in the experiment.

The standard deviation showed that there was no there was no sign of flocculation that would have resulted in significantly worse coloristic characteristics.

Discussion of the Results

There is no significant difference with regard to the coloristic data achieved among the tested binders. The jetness levels reached are remarkably high and definitely can still be improved with the help of specially developed dispersion resins. One detects, however, the influence of the various pigment blacks on the jetness.

Grinding with Dispersion Resins and Wetting Agents

Another experiment was conducted using the dispersion conditions described prior. Table 3 shows the raw materials and coloristic data of the mill base and the black coatings. As was clearly demonstrated, the black paints were only gradually improved by combining the binder and wetting agent in the mill base. An explanation for this could be a competitive situation between the binder and the wetting agent on the pigment black surface. Viscosity of the mill base diminished in all systems. This is of great importance in practice.

Grinding with Wetting Agents

With the development of highly effective wetting and stabilizing agents for aqueous paints, it has become possible to wet and stabilize very fine pigments with a large specific surface area. Pigment blacks manufactured by the furnace black process have a hydrophobic nature, while pigment blacks produced by Degussa's gas black process are hydrophilic and thus differ in the amount of adsorbed wetting agent as well as the adsorption mechanism. By virtue of the surface chemistry, most carbon blacks are negatively charged. Therefore, cationic or neutral wetting agents are preferentially adsorbed by the carbon black.

A low pH of a pigment black is not a reason for not using it in waterborne paints. One merely has to take into account that, due to the low pH, more neutralizing agent is required during the dispersion process. For this reason, the pH of the mill base must be raised by one-half to one point, as compared with what the desired pH should have been after the dispersion process.

Wetting Agent Proportions

One can find in the literature wetting agent proportions in relation to the pigment black surface area between 1-2 mg per m2. For the pigment black FW 285 with a BET surface area of around 350 m2/g, that would mean about 350 mg of wetting agent per g, which would correspond to 35% of wetting agent (active substance). Numerous tests, however, have shown that with fine pigment blacks in most cases1 50% of wetting agent -related to the pigment black - must be used. With pigment blacks having a smaller surface area, the aforementioned values apply.

The pigment blacks' typical morphology, which is dependent on the production process, could be an explanation for this.

Mill Base Formulation

In many experiments, the procedure shown in the above scheme proved favorable in the production of the mill base.

Dispersing was made with a pearl mill. For most experiments, a Skandex disperser BS 20 was used. At the same time, several experiments were additionally carried out with the mini-zeta laboratory pearl mill (Netzsch), and the results were confirmed. These results cannot be generalized, because a pearl mill shows a higher efficiency in other formulations

With increasing dispersion time, the following occurs.

    Gloss at 20 deg increases
    Haze decreases
    Jetness My increases to a certain degree
    Hue dM becomes bluer with better stabilization of fine pigment
    Grindometer value decreases and shouldbe less than 10 microns


Wetting Agents

The wetting additives have been tested and were found to be particularly efficient in comparison to others. The wetting agent concentrations are between 50% and 100%, related to the pigment black. XPB FW 285, with an average primary particle size of 11 nm and a concentration of 10% - related to the binder - was used as the pigment black. Letting down was carried out with Alberdingk U 710 (see Figure 4).

Figure 5 shows differently strong interactions of the dispersion additives with various pigment blacks, which can be seen especially with the hue - an obvious criterion for stability.

Discussion of the Results

As shown in Figures 4-5 in comparison to Table 3, the level of coloristic data is higher than that achieved with the pure grinding with dispersion resins. The described procedure is, however, not always possible since a lot of water is added to the finished paint through the milling formulation. One can try to increase the concentration of carbon black in the mill base or directly incorporate the pigment black.

Influence of the Let-Down Resin

The tests carried out under identical conditions show the gradual difference in coloristic data depending on the let-down resin. The better the stabilization of the carbon black in the mill base, the less the tendency towards flocculation during the let-down process. The sequence of the addition of raw materials is just as important to the let-down process as it is to the preparation of the mill base (see Table 4).

Following are a few rules of thumb for the let-down process.

  • Ensure that the raw materials to be mixed have a good compatibility over the whole range of concentration.

  • Adapt the pH of the mill base and the let-down resin.

  • The temperature difference between the mill base and the let-down components should not be too large.

  • If possible, the raw materials should be added while stirring constantly.

  • If co-solvents must be employed, they should be grinded already with the mill base.
Dependency of the Coloristic Data on the Pigment Black Concentration

As expected, the jetness and, to a smaller extent, the bluish tint increase with an increasing concentration of the pigment black (see Figure 6). However, here again, we wish to refer to the logarithmic nature of the My value. If one takes reflection as the base, jetness tends to approach an asymptote with increasing pigment black concentration. Of course, the pigment black concentration in a mill base primarily is limited by the rheology.

For more information on pigment black, contact Maria Nargiello-Tetreault, Applications Manager, Degussa Corp., Akron Technical Center, 3500 Embassy Parkway, Suite 100, Akron, OH 44333; phone 888/SILICAS; e-mail maria.nargiello-tetreault@degussa.com; or Circle Number 96.

Brief Description of Pigment Blacks

Pigment Black XPB FW 285 has the deepest jetness among the carbon blacks manufactured by Degussa for waterborne paints. The well-known advantages of the Degussa gas blacks such as good dispersibility, high gloss and low haze in finishing paints are also especially strongly pronounced with FW 285. Due to its slightly acidic pH, the pH drop during dispersion is slight and pH stability is excellent.

Pigment Black FW 1 falls under the same category, being likewise a gas black with all the positive characteristics mentioned earlier. In its coloristic data, it exhibits somewhat less jetness than XPB FW 285.

FW 200 and FW 2 belong to the group of additionally treated gas blacks.

The starting carbon black FW 1 is oxidized, with FW 200 being more oxidized than FW 2. Their strengths lie in the solvent-containing systems. With certain prerequisites followed, they can also be used in waterborne paints, exhibiting in them coloristic data much similar to those of FW 285. Due to the differing surface chemistry, other wetting agents and wetting agent concentrations could bring better results as against the non-oxidized carbon blacks. Since the pH is relatively low, higher amounts of neutralization agent are necessary in comparison to FW 285.

Colour Black S 170 is comparable to FW 1 in terms of surface chemistry but it is less fine and, therefore, exhibits somewhat less jetness. However, it is economically interesting.

Special Black 4 (ox.) and Printex U / Printex V are the so-called all-around carbon blacks, and are popular all over the world. They are used as much in waterborne paints as in conventional systems for black and gray coatings. Although they are relatively fine, they do not tend to a pronounced "rub-out" effect. They are especially preferred in one-coat paints since a high gloss and very good hiding power can be obtained with relatively good dispersibility.

Flame Black 101, Printex G and Special Black 100 have proven themselves well as pure tinting blacks. Printex 200, similar to tinting blacks, is relatively coarse for a pigment black and due to its relatively low conductivity in water it is predestined to be used in electrodeposition paints.

References

1 Mathias J., Lippok-Lohmer K., Welt der Farben 10/97, 28.
2 Lippok-Lohmer K., farbe+lack 92 (11), 102h (1986).
3 Coatings Comet February 1999, 36-37 (IRFARB).
4 What is carbon black, Firmenschrift der Degussa AG, Frankfurt 1999.
5 Ferch H., Pigmentru?e, Vincentz Verlag, Hannover 1995.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Paint and Coating Market Reports
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • Off-Diagonal Effects of Alkanolamines in Waterborne Coatings

    See More
  • The Use of Aqueous Pre-Dispersed Fumed Silica to Improve Film Formation in Waterborne Coatings

    See More
  • Study Predicts Rise in Waterborne Coatings in the Protective and Specialty Markets

    See More

Related Products

See More Products
  • Pigment Dispersion (Virtual Course - 11/19/26)

See More Products

Related Directories

  • Schlenk Metallic Pigments

    SCHLENK supplies state-of-the-art metallic pigments, including solvent and waterborne aluminum and gold bronze pigments for all coatings and paint applications. In addition, we supply unique special effects like our Zenexo® ultra-thin colored aluminums that offer unmatched durable gold and orange effects. Our very broad Decomet® vacuum metallized pigment line allows formulators to achieve very smooth metal and chrome-like effects. SCHLENK products are available globally.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing