Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

Plate-Like Pigments in Automotive Paints: a Review

April 26, 2002
In recent years, automotive colors have become an important aspect of car design. Market experience shows that car buyers tend to prefer automotive coatings with high chroma shades based on effect pigments because of their visual impact.1 For creation of clearer, more brilliant and more exciting colors for automotive original equipment manufacturers (OEM) finishes the number of pigment types used has therefore increased considerably in the last decade. An end to this trend is not yet in sight.

In addition to conventional "one-dimensional" organic and inorganic pigments, which interact with light by absorption and/or scattering, more "two- and three-dimensional" plate-like pigments are finding their way onto the market.2 The optical impression of these pigments is based on three kinds of interaction of light. First, if they consist only of small metallic flakes with diameters more than five micrometers the incident light is almost all directly reflected. That means these pigments act as small mirrors, which results in a lightness flop with change of the viewing angle. The "dollar" and "corn flake" types of aluminum pigments belong to this "two-dimensional" pigment group.

Second, if the plate-like particles are based on, or contain, selectively absorbing materials the interaction with light is based on absorption and reflection. As a result, both the reflected and the transmitted light are colored. Plate-like iron oxides (e.g., BASF Paliocrom Copper L 3000 and L3101) and plate-like phthalocyanine (BASF Paliochrom Blue Gold L 5000) belong to this group.

If plate-like pigments with diameters of more than five micrometers contain or are based on thin films with a thickness in the range of the visible light, interference and reflection effects are generated. This third interaction of light is well known for the "three-dimensional" plate-like pearlescent pigments based on highly refracting materials like bismuth oxychloride and titanium oxide-coated micas.3

Most interference (pearlescent or luster) pigments now consist of at least three layers of two materials with different refractive indices. Thin flakes (thickness ca. 500 nm) of a material with a low refractive index (mica) are coated with a highly refractive metal oxide (e.g., TiO2, layer thickness ca. 50-150 nm). This results in particles with four interfaces. More complex multilayer pigments containing additional thin (e.g., light absorbing) films have also been produced and can be found in OEM paints.4

Interference (pearlescent or luster) pigments split white light into two complementary colors that depend on the platelet thickness. The interference color dominates under maximum reflection (face angle). The transmitted part dominates at other viewing angles under diffuse viewing conditions provided there is a white (non absorbing) or reflecting background. Variation between face angle and grazing angle for incident rays therefore produces a sharp gloss peak and a color change between two extreme complementary colors (color flop).

Against a black background or in a blend with carbon black (a frequent situation in the basecoats of two-coat paint systems), the transmitted light is absorbed and the reflected interference color is seen as the mass tone of the material. In combination with absorption pigments two-tone effects can be achieved if the absorption color differs from the interference color. The optical impression of plate-like pigments with diameters of more then five microns can be described by the Fresnel equation.

In general the reflection is a function of the refractive index (n) and the absorption constant (k) of the material, the wavelength of incident light (l) and the irradiation angle (e) R=f (n,k,l,e). In a simplified form (e=90?, k=0) the Fresnel equation is:

This equation clearly shows that the greater the difference between the refractive indices of the plate-like pigment (n2) and the binder (n1), the greater the reflection and, accordingly, the gloss of the pigment. This is why the pigment industry prefers highly refractive materials. But the angle-dependent color play observed in thin films of such materials is restricted. In contrast thin films of inorganic materials with low refractive indices like SiO2 or MgF2 (so called dielectric materials) show like soap bubbles strongly angle-dependent color hues. This real color play of such materials can be explained by Snell's Law.

Snell's Law correlates the refractive angles and the refractive indices. In the case of a highly refractive material like TiO2 light rays at a face angle and grazing angle are refracted close to the perpendicular. In the case of SiO2 bending toward the perpendicular is low. As a result the interference conditions for face and grazing angle rays are completely different and strongly angle-dependent colors are obtained. The best materials for optical variable (OV) pigments therefore would be flakes of SiO2.

However, there is one problem. It can be calculated from the simplified Fresnel equation that the reflection of light on a thin solid film with low refractive index is weak.

The solution is to strengthen the reflection - and thus the chroma - by surrounding the non-absorbing dielectric with a very thin semi-transparent layer of highly reflective material.

By doing this, the extent of extinction and enhancement of particular wavelengths is efficiently increased. These OV pigments therefore exhibit deep colors, high gloss and a high color dependence on the viewing angle (color flop). So far, OV pigments of the Fabry-P?t type and OV pigments with inner reflector are on the market. The Fabry-Parot type has a dielectric core of low refractive material, which is surrounded by a semitransparent reflector.5

The inner reflector type has a core of reflecting material, which is surrounded by a symmetrical system of weakly refracting and highly reflecting layers.

This example shows the color flop in the Al/SiO2/Fe2O3-system.

So far, OV pigments are produced only by Flex Products Inc., Merck6-7 and BASF. Recently holographic pigments have added a new dimension to paint. To create these pigments a specific holographic light recording is embossed in 50-100 ?m particles cut from 12 micrometer polyester film.8 PPG Industries is marketing this new product under the trade name Geometric PigmentsTM. BASF Corp. will soon introduce these pigments to the OEM market.

Another concept is the creation of interference pigments on the basis of liquid crystals (Wacker-Chemie AG, BASF AG).9

In addition to these interference pigments micro titanium dioxide must not be forgotten. This ultra fine material (particle size ca. 10-50 nm) is found more frequently in the basecoats of two-coat metallic systems since its introduction in 1987, as it is also possible to obtain a color flop with this product.10

A new generation of effect pigments is represented by aluminum pigments coated with color pigments. The organic or inorganic color pigments are permanently fixed on the flake surface by a layer of silicon dioxide. Compared to the same pigmentation level in conventional metallic coatings ALUCOLOR(r) in blue and green (Eckart-Werke, Germany) provides higher color strength. The blue flop of ALUCOLOR white creates a stainless steel surface finish.

Colored aluminum pigments are also produced by Showa Aluminum Powder K.K. Japan and distributed under the trade name Fireflake. Six colors are available in four particle size ranges. A new class of aluminum pigments are the ALOXAL(r) pigments from Eckhart-Werke Germany. The "champagne-colored" shades of ALOXAL generate warmer and deeper metallic effects with good brilliance and opacity.

Conclusion

Plate-like pigments have visual, physical and chemical advantages. Applications for these pigments include not only cars but also building exteriors, furniture, and cosmetics. Therefore, the forensic scientist is becoming confronted with plate-like pigments more frequently. Several new plate-like pigments will come onto the market soon, including OV pigments of the Fabry-P?t type, inner reflector type, liquid crystal type and holographic pigments.

A concept for classifying and identifying plate-like pigments by applying a combination of analytical methods has been published. 11

References

1 Novinski, S.J.; Nowak, P.J.; Venturini, M.T. Pearlescent Pigments in High Performance Coatings. Presented at Intertech Conference; 1997 Oct. 27-29, Chicago

2 Esselborn, R.; Franz, K.D.; Hofmeister, F. Color Styling with Lustre Effect Pigments in Multi-Layer Systems. Presented at the Eurocoat 85 Congress; 1985, Stra?burg

3 Franz, K.D.; Emmert, R.; Nitta, K. Interference Pigments. Kontakte (Darmstadt). 1992; 2:3-14. ISSN 0172-8717

4 Teaney, S.; Denne, I. Color Formulations with Iriodin(r) / Afflair(tm) Pigments for Automotive Coatings. Kontakte (Darmstadt). 1992; 2:46-55. ISSN 0172-8717

5 Schmid, R.; Mronga, N.; Radtke, V; Seeger, O. Optically Variable Lustre Pigments - Optisch variable Glanzpigmente. Farbe & Lack. 1998;104:44-48.

6 Sharrock, S.R.; Schuel, N. New effect pigments based on SiO2 and Al2O3 flakes. European Coatings J. 2000;1. http://www.coatings.de/papers-archive.cfm.

7 Kuntz, R.F.; BrAckner, H.D. Pearl Lustre Pigments with Improved Properties. Presented at the 3rd NArnberg Congress; 1995 March 13-15, NArnberg

8 Anon. Holographic Pigments - Add New Dimensions to Paint. PCI. 1997:48-49.

9 Heinlein, J.; Kasch, M. Pigments Offer Color Effects Matched Only by Nature. PCI. 1999:58-75.

10 Winkler, I.; Proft, B. Vor UV schAtzen und selektiv blaues Licht streuen - Eigenschaften und Anwendungen von nanokristallinem Titandioxid. Farbe & Lack. 2001;107:28-36.

11 Stoecklein, W. The Analysis of New Plate-Like Pigments in Automotive Coatings. PCI. 2001: 48-65.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • The Analysis of New Plate-Like Pigments in Automotive Coatings

    See More
  • A Review of Compulsory Coatings Standards in China

    See More
  • A Review of Global Supply and Demand for Titanium Dioxide

    See More

Related Products

See More Products
  • Automotive Paints and Coatings, 2nd Edition

  • Failure Analysis of Paints and Coatings, Revised Edition

See More Products

Events

View AllSubmit An Event
  • February 24, 2026

    Implementing AI in Paints & Coatings: Doing It Right

    On Demand This webinar is designed for Enterprise Paints and Coatings leaders (Innovation, R&D, Product, Production) tasked with introducing AI, whether they are unsure where to start or have already launched pilots but struggle to scale. Attendees will learn common pitfalls of AI adoption and how experienced partners enable confident, scalable, and measurable impact in global Enterprise organizations.
View AllSubmit An Event

Related Directories

  • Schlenk Metallic Pigments

    SCHLENK supplies state-of-the-art metallic pigments, including solvent and waterborne aluminum and gold bronze pigments for all coatings and paint applications. In addition, we supply unique special effects like our Zenexo® ultra-thin colored aluminums that offer unmatched durable gold and orange effects. Our very broad Decomet® vacuum metallized pigment line allows formulators to achieve very smooth metal and chrome-like effects. SCHLENK products are available globally.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing