Powder Coatings Offer Global Opportunities for Coatings & Raw Material Manufacturers



The 2001 global thermosetting powder coatings market of over 900,000 tonnes is valued at approximately EUR 3.6 billion (US$ 3.2 billion). Europe leads the way with approximately 43%, Asia 26%, North America with 23%, and the rest of the world with 8%. Penetration of powder coatings differs by country and region from 4% up to 15%.

Irfab reports there is still plenty of room for increased penetration of powder coatings in the world paints arena.

With growth rates that vary by region from 4.5-10% per year, by the year 2003, the global powder coatings market will reach the one million tonnes (2.2 billion lbs) mark.

Polyester-epoxy hybrids dominate the powder coatings industry, representing on a global scale approximately 55% of the market, followed by polyesters, epoxies, polyurethanes and acrylics.

Average country or regional prices across the board vary considerably, from highs of approximately EUR 6.40/kg to EUR 2.30/ kg. In certain areas prices are in free fall.

These are some of the striking conclusions from a strategic market and technology assessment study conducted by Irfab Chemical Consultants, sponsored by major chemical and liquid and powder coatings companies worldwide. The study, "Powder Coatings Europe 2001-2010 - A Global Comparison: Europe, Americas, and Asia," covers more than 50 countries and 200 manufacturing sites globally.

After the turmoil in the global markets during 2000-2001, Irfab recognized the need to re-appraise several market segments. In compiling this report, great attention has been given to the correct 2001 data input. This has resulted in a true and realistic 2001 situation and forecast of growth in this global market to the year 2010.

The study deals with low-temperature and radiation-curing powders, e.g., on wood and other temperature-sensitive substrates, thin-film technology, high-speed continuous coil coating, pre-cut metal blanks, and automotive OEM. It provides market information by country, application segment and type of chemistry; consumption of raw materials; novel TGIC replacement curing agents; and company profiles of both powder coatings manufacturers and raw material suppliers. Selected product literature from raw materials manufacturers worldwide is provided as an attachment.

The differentiated penetration of powder coatings compared to low-solids, high-solids solventborne, waterborne and radiation-curable coatings in the different regions of the world is presented.

This study bears all the usual trademarks of an Irfab report, allowing for concise and accurate forward planning by industry leaders in global markets.

The report is useful for corporate business and R&D decision makers, and provides tools for strategic decision-making to identify untapped opportunities and explore new geographical markets.

Irfab Chemical Consultants is a global marketing consultancy company, involved exclusively in highly specialized market assessment and long-term technology forecasting in the coatings sector and related raw materials. For more information, contact Irfab, 24 J.B. Denayerstraat, 1560 Hoeilaart (Brussels), Belgium; phone + 32 2 657 35 85; fax 32 2 657 90 21; visit www.irfab.com; or e-mail franco.busato@irfab.com.

Links

You must register or login in order to post comments.

Multimedia

Videos

Image Galleries

Podcasts

PCI Top 5 - January 12, 2012
PCI's Podcast series on the five most e-mailed/shared articles and stories for the week.

More Podcasts

THE MAGAZINE

PCI Magazine

February 2012 cover

2012 February

PCI's new issue is now available. Check it out!

TABLE OF CONTENTS SUBSCRIBE

Coating Technology

What resources do you refer to when learning about coatings technology?
See Poll Results Poll Archive

THE PCI STORE

Power Coatings
CD Verison: Powder Coatings - Foundation for the Novice Formulator by Kevin Biller for $29.95 plus shipping
ON CD - Powder Coatings have been the fastest growing finishing technology for the past 30 years. In spite of this tremendous growth and the technology advances that come with it, very few technical tools have been provided for the formulator.
More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Virtual Brochures

PageCollageClick to the Virtual Brochures page to view multiple catagories that list downloadable product literature from leading industry suppliers.

STAY CONNECTED

Facebook Twitter  LinkedIn