Breaking News

Researchers Create Freestanding Nanoparticle Films

Nanoparticle films are no longer a delicate matter. Vanderbilt University physicists have found a way to make them strong enough so they don’t disintegrate at the slightest touch.

NASHVILLE, TN - Nanoparticle films are no longer a delicate matter. Vanderbilt University physicists have found a way to make them strong enough so they don’t disintegrate at the slightest touch.
 
In the last 25 years, scientists have come up with a number of different methods to mold nanoparticles into thin films. These films have a variety of interesting potential applications, ranging from semiconductor fabrication and drug delivery to solid-state lighting and flexible television or computer displays.
 
Until now, these films have had a common problem: lack of cohesion. Nanoparticles typically consist of an inorganic core coated with a thin layer of organic molecules. These particles are not very sticky, so they don’t form coherent thin films unless they are encapsulated in a polymer coating or mixed with molecules called chemical cross-linkers that act like glue, sticking the nanoparticles together.
 
“Adding this extra material can complicate the fabrication of nanoparticle films and make them more expensive. In addition, the added material, usually a polymer, can modify the physical properties that make these films so interesting,” said James Dickerson, Assistant Professor of Physics at Vanderbilt University. Dickerson headed the research group that developed freestanding nanoparticle films without any additives.
 
The properties of the new films and the method that the researchers use to create them are described in the article, “Sacrificial layer electrophoretic deposition of freestanding multilayered nanoparticle films,” published online in the journal Chemical Communications. “Our films are so resilient that we can pick them up with a pair of tweezers and move them around on a surface without tearing,” said Dickerson. “This makes it particularly easy to put them into microelectronic devices, such as computer chips.”   
 
Dickerson considers the most straightforward applications for his films to be in semiconductor manufacturing to aid in the continued miniaturization of digital circuitry and in the production of flexible television and computer screens.
 
A key component in the transistors in integrated circuits is an insulating layer that separates the gate, which turns current flow on and off, from the channel through which the current flows. Traditionally, semiconductor manufacturers have used silicon dioxide for this purpose. As transistors have shrunk, however, manufacturers have been forced to make this layer thinner and thinner until it reached the point where electrons leak through and sap the power from the device. This has led semiconductor manufacturers to retool their process to use “high-k” dielectric materials, such as hafnium oxide, because they have much higher electrical resistance.
 
“We have made high-k nanoparticle films that could be cheaper and more effective than the high-k materials the manufacturers are currently using,” Dickerson said.
In addition, Dickerson argues that the films have properties that m
ake them ideal for flexible television and computer screens. They are very flexible and don’t show any signs of cracking when they are flexed repeatedly. They are also made using a technique called electrophoretic deposition (EPD) that is well suited for creating patterned material and is compatible with fluorescent materials that can form the red, green and blue pixels used in flat-panel television screens and computer displays.
 
EDP is a wet method. Nanoparticles are placed in a solution along with a pair of electrodes. When an electric current is applied, it creates an electrical field in the liquid that attracts the nanoparticles, which coat the electrodes. Using colloids, mixtures with particles 10 to 1,000 times larger than nanoparticles, EDP is widely used to apply coatings to complex metal parts such as automobile bodies, prosthetic devices, appliances and beverage containers. It is only recently that researchers like Dickerson have begun applying the technique to nanoparticles.
 
“The science of colloidal EDP is well known, but the particles are substantially larger than the solvent molecules. Many nanoparticles, however, are about the same size as the solvent molecules, which makes the process considerably more complicated and difficult to control,” Dickerson explains.
 
To get the method to work, in fact, Dickerson and his colleagues had to invent a new form of EDP, which they call sacrificial layer electrophoretic deposition. They added a spun-cast layer of polymer to the electrodes that serves as a pattern that organizes the nanoparticles as they are deposited. Then, after the deposition process is completed, they dissolve (sacrifice) the polymer layer to free the nanoparticle film.
 
According to the researchers, films made in this fashion stick together because the electrical field slams the nanoparticles into the film with sufficient force to pack the particles together tightly enough to allow naturally attractive inter-particle forces to bind the particles together.
 
So far, the Dickerson group has used the technique to make films out of two different types of nanoparticles: iron oxide and cadmium selenide. They believe the technique can be used with a wide variety of other nanoparticles.
 
“The technique is liberating because you can make these films from the materials you want and use them where you want,” Dickerson said.
 
The co-authors on the paper are graduate students Saad A. Hasan and Dustin W. Kavich. The research was funded by a grant from Vanderbilt University.
You must register or login in order to post comments.

Multimedia

Videos

Image Galleries

American Coating Show 2012

The American Coatings Show and Conference, held every two years, took place May 7-10 at the Indiana Convention Center in Indianapolis, IN, in the heart of the Manufacturing Belt, the oldest and largest concentration of industrial companies in the Midwest.

Podcasts

PCI Top 5 - January 12, 2012
PCI's Podcast series on the five most e-mailed/shared articles and stories for the week.

More Podcasts

THE MAGAZINE

PCI Magazine

PCI may 2012 cover

2012 May

Check out PCI's May issue!!

TABLE OF CONTENTS SUBSCRIBE

iPad

Do you own/use an iPad?
If yes, do you use your iPad for business or personal reasons?
Have you purchased a business app within the last 6 months?
See Poll Results Poll Archive

THE PCI STORE

PCI-June-2011-Coversmall.gif
PCI Additives Handbook

Encyclopedia of information on the properties and uses of coatings additives.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Virtual Brochures

PageCollageClick on the Virtual Brochures page to view multiple categories that list downloadable product literature from leading industry suppliers.

STAY CONNECTED

Facebook Twitter  LinkedIn YouTube