ASHLAND, MA - After a three-year startup period, the Schlenk Group has begun operation of a production site for aluminum pigments in Taixing, China. Schlenk Metallic Pigments will produce and distribute its current range of high-performance metallics at the site. The onsite laboratory equipment and quality control procedures at the new facility meet the international standards of the Schlenk Group.