Two New Pigments
Hoover Color Corp. offers two new pigments, Hoover 320bs burnt sienna and P-250 natural red. 320BS burnt sienna is a dark, warm sienna, with as much as 50% increased tinting strength over conventional burnt siennas available today. It is recommended for use in wood finishes and art materials. P-250 natural red is a high chroma, low-cost iron oxide, and finely ground for use in high-speed dispersion equipment. It is a general use pigment for use in all applications, particularly metal primers. Circle No. 238