Q-Lab Technical Marketing Specialist Appointed Vice Chair of ISO Standards Committee
WESTLAKE, OH – Weathering testing company Q-Lab announced that Sean Fowler, a Technical Marketing Specialist at the company, was recently appointed Vice Chairman of the U.S. Technical Advisory Group of TC156 for ISO. This group focuses on the corrosion of metals and alloys.
Some of the corrosion standards covered by this committee include ISO 9227 (corrosion tests in artificial atmospheres – salt spray tests) and ISO 16701 (accelerated corrosion in an alternating conditions of controlled humidity and salt spray).