YANTAI, China - Wanhua Chemical Group announced the successful start-up of the company’s new IPDI plant. Wanhua will be the first Asia-based company to employ the complete IP-IPN-IPDA-IPDI industry chain technology.
The new plant is located in Wanhua’s 10-square-mile Yantai Industrial Park. With the latest phosgene production technology and a fully integrated supply chain, the new state-of-the-art plant strategically places Wanhua in this market. Wanhua will market the IPDI monomer under the brand name WANNATE®.