King Introduces Several New Additive and Resin Technologies
King Industries is featuring multiple new products at Booth 2171. NACURE® XC-320 is a new and novel catalyst designed for automotive OEM coatings, metal decorating, coil coatings and general industrial coatings. It provides rapid cure response in both water- and solvent-based coatings. Formulations baked for 20 min at 120 °C (250 °F) demonstrate fast cure speed in comparison to conventional acid catalysts. The light color of this catalyst allows for use in clear coats and light color pigmented systems.
In addition, a new NACURE catalyst has been developed to accelerate the cure of ambient or baked coatings based on the Dow Paraloid™ Edge technology (carbamate/dialdehyde chemistry).This catalyst provides improved adhesion to metal substrates and high moisture and corrosion resistance performance.