AkzoNobel has launched an ultrareflective powder coating that can increase the effective output of commercial lighting fixtures by up to 30 percent. Developed by the company’s Powder Coatings business, Interpon ReFlex delivers outstanding levels of light reflectance, which make it very cost effective. What’s more, because the product is solvent-free (like all powder coatings), it also has a lower environmental impact than competing materials used in the lighting market.
“Interpon ReFlex allows you to obtain more light from a specified power input for any light source, including halogens and LEDs,” explained Mark Reekie, Global Marketing Manager, General Industrial at AkzoNobel Powder Coatings.