Toyo Ink Selected as Preferred UV Ink Supplier to KBA-Sheetfed
TOKYO - Toyo Ink Co. Ltd., a wholly owned subsidiary of the Toyo Ink Group, was chosen as the preferred global supplier of UV sheetfed offset inks to KBA-Sheetfed Solutions AG & Co. KG, a business unit of the Koenig & Bauer Group of Germany.
The FLASH DRY™ series from Toyo Ink—the standard FLASH DRY Karton series, the energy-conserving FLASH DRY HS series and the FLASH DRY LED series—will be the recommended UV inks for KBA-Sheetfed’s UV presses. These three inks will continue to be available exclusively from the Toyo Ink Group’s dealer network.