Graphene Nanoplatelets from Applied Graphene Materials
Adding graphene nanoplatelets to epoxy coatings has shown outstanding performance enhancements across industry ISO-standard anticorrosion and barrier tests. Tests demonstrated that very small additions of this product decreased water vapor transmission rates by up to 95% and extended time to initial corrosion in excess of 500%. E-mail richard.akam@appliedgraphenematerials.com.