LONDON – Synthomer announced price increases on acrylic-, styrene- and butadiene-based dispersion and latex products.
The company will raise prices on a per-tonne (wet) basis in Europe on the following products: pure acrylics up to €100, styrene-acrylics up to €150, carboxylated styrene-butadiene up to €200, and any other butadiene-containing product up to €300.