Sherwin-Williams’ Powder Topcoats Earn Army Research Lab Approval
CLEVELAND – Sherwin-Williams, through its Product Finishes Division, announced the U.S. Army Research Lab has approved MIL-PRF-32348 Type III, Class I Chemical Agent Resistant Coating (CARC) Powder Topcoat in Black 37030, Green 383 34094 and Tan 686A 33446 for registration on the Qualified Products Database, and may be applied to any military asset.
Designed to work with a primer to provide coverage and corrosion resistance to coated parts, these high-performance, near-zero-gloss CARC powder topcoats help safeguard American military vehicles and the warfighters within through chemical agent resistance and protection from detection through an infrared signature. The coatings have been field tested to stand up to the most rigorous conditions.