WACKER Begins Construction of Pyrogenic Silica Plant in Tennessee
ADRIAN, MI/CHARLESTON, TN – Wacker Chemie AG, the Munich-based chemical group, officially started construction on its HDK® pyrogenic silica plant, which is located adjacent to WACKER’s Charleston, Tennessee, polysilicon plant. The groundbreaking ceremony was attended by representatives from politics, business and local government. WACKER Executive Board Member Auguste Willems, State of Tennessee dignitaries and local officials broke ground for the new plant. Annual capacity of the new facility will be 13,000 metric tons, and completion is scheduled for the first half of 2019.
“With the USA being the second-largest chemical market, the Charleston, Tennessee, HDK pyrogenic silica plant will enable WACKER to keep pace with growing demand for this indispensable product,” said Willems. “This new facility is a key component of Charleston’s supply chain. It is the next step toward expanding Charleston into a fully integrated silicon site,” he explained.