Wageningen University & Research and IPSS Engineering Launch Anti-Solvent Technology
WAGENINGEN, the Netherlands – Wageningen University & Research (WUR) and IPSS Engineering (IPSS) have signed a long-term cooperation agreement for the further development, optimization and commercialization of the new anti-solvent crystallization technology ProKris.
Both parties have been cooperating in this field in a number of projects since 2014. Currently, a project with the objective to build the first pilot installation for the ProKris technology is running, focusing on results by the end of this year. IPSS Engineering will realize this pilot installation in a dedicated technology hall, situated in the Plus Ultra building on the Wageningen Campus.