PITTSBURGH – PPG introduced PPG DURASTAR® ultra-durable industrial spray coating, a one-coat application for aluminum extrusions that meets the exterior durability requirements of the American Architectural Manufacturers Association’s AAMA 2604 specification (five-year South Florida exposure).
Composed of a proprietary PPG-developed polyester resin, PPG Durastar spray coating can be applied direct-to-metal (DTM) or over a primer. It provides excellent corrosion resistance, color fastness, and chalk-, scratch- and mar-resistance for high-end building products and components used in storefronts, schools, hospitals and other high-traffic areas.