Terrazzo flooring is a composite – a mix of resin with aggregates, which give the product such variety in its design.
Intended to be a durable, hard-wearing and highly decorative flooring solution, the resin is mixed with colored marble, granite chips or other approved aggregates such as glass. During production, the mix is ground and polished to reveal the pattern of the aggregates, which contrasts with the colored epoxy.