TORONTO — DCC LANSCO® is installing a new production line for the manufacture of organic pigments in order to meet increasing market demand for the company’s products, which will increase capacity by more than 50%.
DCC LANSCO’s high-performance Benzimidazolone, Metal Salt Azo & Hansa yellow pigments have been further developed to better meet the increased technical demands of the coatings and plastics markets. These products have been engineered for excellence in performance, creating additional value for the customer.