Master Painters Institute Announces New Product Standards
HOUSTON - The Master Painters Institute (MPI), a division of the NACE International Institute, announced its completion of product standards for interior carbon-steel fuel pipes, interior welded fuel tanks, exterior steel systems, and waterfront steel structures. MPI was contracted by Naval Facilities Engineering Command to establish the product standards.
The new MPI 500 Series Standards are for use in numerous aspects of work involving specialized Department of Defense petroleum, oils, and lubricants facilities. Initial testing is now complete, and the standards are available via the online MPI store. Coatings manufacturers can submit products for approval beginning in May 2019.