Acrylic Emulsion from Engineered Polymer Solutions
EPS® 719 is an all-acrylic emulsion designed to minimize asphalt bleed-through in cool roof coatings while maintaining flexibility and toughness. It is flexible at temperatures as low as -10 °C, offers dirt pickup and UV light resistance, and provides excellent toughness with both high tensile strength and elongation. Visit epscca.com.