Powder coatings have always offered customers numerous environmental benefits - now they've become even more sustainable following the launch of a full range of Interpon Low-E products developed by AkzoNobel.
The company introduced its first Low-E products — a coarse texture range — late last year. Now a complete range of smooth finishes in Interpon 610 has been added to the Low-E portfolio. Specially engineered for curing at temperatures lower than the current standard of 180-190 °C, the new offering is TGIC-free polyester, which saves energy and helps customers to improve their efficiency.