Cortec® has again met the demands of an ever-changing regulatory landscape, now with the successful reformulation of MCI® POWR 100, a powerful three-in-one concrete surface treatment for water repellency, oil and stain resistance, and corrosion protection. This multi-functionality makes MCI POWR 100 particularly beneficial for commercial buildings, parking garages, bridges and industrial floors exposed to high levels of oils, greases or water.
MCI POWR 100 works in three ways. First, the silane component of MCI POWR 100 provides water repellency by chemically reacting with the cementitious substrate under proper application, decreasing the ingress of aggressive materials. Second, an oleophobic additive modifies the concrete surface to increase resistance to oil and food stains. Third, the MCI component penetrates deep into the substrate, forming a protective, molecular barrier on embedded reinforcement to reduce the rate of corrosion at the rebar surface.