Contractors Enjoy Unrivalled Benefits with Revolutionary Fire Protection Coating
The increasing demands made by architects and designers creating the striking steel structures rising in our towns and major cities travel through the supply chain all the way through to the contractor. For the application of passive fire protection coatings, the contractor needs to be assured that the coating can be applied efficiently without downtime and that it satisfies the agreed requirements of the original specification without compromise, with considerations of speed of construction and occupancy of the building.
In the civil construction industry, most intumescent coatings typically dry by a process of water or solvent evaporation, and when applied at a high film thickness can take some time in the process. In response to the industry’s growing concerns about downtime and time savings, the Sherwin-Williams Innovation and R&D teams have developed the second generation of revolutionary technology under the FIRETEX® FX6000 series.