South Australian Technology Start-Up Researches Nanomaterials
NORWOOD, Australia — Two South Australian companies have joined forces to create a start-up specializing in the research and development of a naturally occurring nanoparticle.
Natural Nanotech Pty Ltd., jointly owned by Minotaur Exploration and Andromeda Metals, will research the conversion of naturally occurring halloysite-kaolin clays into high-value nanomaterials.