ZURICH – DKSH Business Unit Performance Materials has become an exclusive partner for Keyland Polymer to grow its presence and market share for its portfolio of resins. The partnership will cover Europe, India, Japan, South Korea, Taiwan, Australia and New Zealand.
Under the agreement, DKSH will provide exclusive distribution for Keyland Polymer’s UV curable resins, with a focus on the powder coatings market. The UV resins are used in powder coatings for metals, plastics, carbon fiber and composites, and are particularly well suited for heat-sensitive applications where process and curing temperatures cannot exceed 130 °C.