SURECO™ AF 2320 from AGC Chemicals Americas is a transparent fluoropolymer coating that repels dirt, oil and water, minimizes fingerprints, and makes surfaces easier to clean. Because of its versatility, SURECO AF 2320 is ideal for glass, metal, plastic and stone surfaces. It is widely used to protect electronics screens, interior architectural surfaces, interior automotive surfaces, granite countertops and ceramic tiles.
SURECO 2320 coatings minimize smudges and enable easy cleaning without altering the appearance of the object’s surface. A thin layer can be applied on a glass or optical surface using a wet process like spray, dip or spin coating or a dry process like vapor deposition. A monomolecular layer (< 10 nm) of SURECO 2320 provides complete, effective surface protection.