Italian Company Pioneers Antiviral Powder Coatings
L’AQUILA, Italy — Stardust Powder Coatings, a manufacturer of powder coatings based in L'Aquila, Italy, has tested, with positive results, an antiviral coating that can inhibit the human Coronavirus NL63.
Powder coatings with antiviral properties are special virucidal coatings for application on metal surfaces. These coatings can inhibit the viruses present on the metal surfaces that surround us, for example furniture and lighting fixtures, thus reducing the risk of the active virus coming into contact with humans due to a contaminated surface.