Coating for Corrosion-Under-Insulation Applications from PPG
PITTSBURGH – PPG recently announced the North American introduction of PPG HI-TEMP 1027™HD coating, which is a next-generation, ambient-cure coating engineered for challenging corrosion-under-insulation (CUI) conditions.
A high-build product that offers dry film thickness of 10 to 12 mils in a one-coat application, PPG HI-TEMP 1027HD coating provides excellent protection against corrosion on pipes, vessels and construction parts when plants are in operation. The highly durable coating is formulated to withstand severe temperature cycles ranging from -320 °F (-196 °C) to 1,000 °F (540 °C) and resists dry exposure with intermittent temperature peaks of up to 1,200 °F (650 °C).