MP55 Antiviral Paint Technology has proven to be effective against human coronavirus SARS–CoV-2. Significantly reducing the viral load on treated surfaces by over 99.54%, it has been demonstrated in tests carried out in accordance with ISO 21702-2019. Applications include treatment of walls, the creation of washable floors and the protection of furnishings. It is a water-based, VOC-free technology that can help lower viral load in environments such as hospitals, nursing homes, gyms and high-personnel facilities.