A high-end, mixed-use property in the Greater Phoenix area was experiencing an extreme screeching noise in its parking garage. The noise was enough to disturb adjacent businesses and residences. After a couple layers of QuietCoat® acoustical coating from PABCO® Gypsum, the noise and vibration were drastically reduced — in essence, going from a screaming, almost overwhelming situation to a tranquil, peaceful environment.