Water-Based Treatment from Oxford Advanced Surfaces
Oxford Advanced Surfaces, a pioneer in the surface preparation of plastic and composite components for painting and lacquering, has developed a new treatment, KOTEFAST™, that reportedly reduces surface preparation time by over 90% compared to the existing approach of sanding. KOTEFAST is available in a water-based formulation, avoiding the need to use solvents in the workplace.
KOTEFAST was tested on a truck panel and the treatment was time recorded at less than 15 minutes. An identical panel took three hours to prepare using the usual method of manual sanding, indicating a time saving of over 90% when using KOTEFAST.