Carboline Co., a global manufacturer of high-performance industrial coatings, recently announced the introduction of Carbocrete 4010, a new fiber-reinforced repair mortar with outstanding application properties for vertical and overhead concrete substrates.
Carboline reports that this innovative product can build up to 4” (10 cm) thick on vertical surfaces to repair and resurface the most deteriorated concrete surfaces. It also offers a quick setting ability that allows it to be topcoated with various Carboline high-performance linings in as little as six hours, making it ideal for job site production.