Nouryon to Increase Colloidal Silica Production Capacity in United States
AMSTERDAM — Nouryon announced plans to expand production capacity at its Levasil® colloidal silica manufacturing facility in Green Bay, Wisconsin, to meet increasing demand from the construction and packaging end-markets. Construction of the facility expansion is expected to be finalized in the second half of 2022.
“The capacity expansion at our manufacturing facility in Green Bay is driven by growing demand for Levasil colloidal silica products in North America,” said Patrick Wilhelm, Vice President of Inorganic Specialties at Nouryon. “We are pleased to support our customers’ growth, which is fueled by large governmental infrastructure projects as well as increasing demand in packaging materials driven by e-commerce.”