Adsil Inc. announced its new HVAC/R coating, MicroGuard1® 3500 (MG1-3500) HVAC/Metals Coating, has surpassed 18,100 hours in ASTM B117 testing with no salt corrosion evident. Adsil reports that this result is an industry best.
MG1-3500 protects well beyond salt corrosion. EIS testing proves superior protection against other corrosives (chemical, UV and pollution). Its advanced no-mix, low-VOC chemistry also provides benefits not seen in other coatings. Inorganic formulation, anti-fungal properties (ASTM G21 rated 0), sustainability (lowers maintenance and life-cycle costs and extends service life of equipment), 9H Pencil Hardness, 5-B Adhesion, 6–8-micron DFT, 180-degree flexibility, and can be installed in the field or at a coating center.