ST. PETERSBURG, FL – Extreme Coatings announced the launch of a new internal diameter High Velocity Oxygen Fuel (HVOF) coating system for oil and gas and industrial components. The company made the announcement at the Offshore Technology Conference in Houston.
The new IDX internal diameter HVOF coating provides a high-performance tungsten carbide nano coating for diameters as small as three inches, lengths up to eight feet, and thicknesses up to 0.015 of an inch. The thermal spray system — consisting of a delivery mechanism and coating material — provides a tungsten carbide, cobalt chrome coating that delivers exceptional abrasion resistance and three times the service life of chrome-plated parts.