Enhance the performance of your epoxy formulations with the newest systems from Westlake Epoxy, formerly Hexion Coatings & Composites
The INFINIUM™ Epoxy System is a lower yellowing, two-component, ambient-cure system with improved hardness development. This system, comprised of EPON LY™ Resin 1810 combined with EPIKURE LY™ Curing Agent 3801, provides excellent epoxy performance and superior overnight cure.
Key features include lower yellowing, faster reactivity, and reduced application costs.