Siegwerk Manufactures New Generation of NC Inks at Fully Automated Production Facility
SIEGBURG, Germany — Siegwerk is now offering a new generation of NC inks for flexible packaging applications produced with state-of-the-art production equipment at its headquarters in Siegburg, Germany.
For the new generation of NC inks, Siegwerk reports the formulations have been optimized to match both the latest production technologies and current market trends. The new NC ink series includes colors and clears and is designed for gravure and flexo printing of all kinds of flexible packaging. The system’s versatility and flexibility make it a genuinely all-purpose solution for surface and reverse printing with lamination applications. “Compared to previous generations, our new series offers an extended functionality, an outstanding quality consistency and optimized rheological properties, significantly improving print results and efficiency,” said Björn Ewig, head of Technology Flexible Packaging EMEA.