AkzoNobel’s Sustainable Chrome Plating Alternative Saves Bike Manufacturer 40% on Energy Costs
AkzoNobel is supporting major European bike manufacturer BiSAN in making the switch from chrome plating to a more cost-effective, energy-efficient, less labor-intensive, and more sustainable Interpon powder coating.
In adopting Interpon Cr, a chrome-effect powder coating with a metallic finish, BiSAN is providing customers and consumers with bicycle frames and associated products that have all of the fabulous appearance and corrosion resistance of chrome plating, but with none of the environmental downsides.