International® Marine Coatings has published a new whitepaper which reveals the high degree of accuracy of its predictive Intertrac® Vision tool to real-life vessel operations by correlating to the speed loss of a globally trading VLCC vessel over a five-year docking period, in line with the principles of the ISO 19030 standard.
International used the forecasting tool to project a 1.4% speed loss over a 60-month in-service period that proved to be in line with actual vessel performance.
Exclusive Insights: Gain access to in-depth insights and best practices for technical solutions for coatings, inks and adhesives formulators and manufacturers. Comprehensive Coverage: Stay informed with the latest news and trends through our videos, podcasts, eNewsletters, webinars, continuing education resources, and a monthly eMagazine. Networking Opportunities: Connect with other industry professionals and leaders through our webinars and online platforms.